We use cookies and other tracking technologies to improve your browsing experience on our website, to show you personalized content and targeted ads, to analyze our website traffic, and to understand where our visitors are coming from.
Introduction to JIS G3458 alloy steel boiler tube standard specifications-CONTINENTAL STEEL CO.,LTD
BLOGS

Introduction to JIS G3458 alloy steel boiler tube standard specifications

Mar 05, 2024

Introduction to JIS G3458 alloy steel boiler tube standard specifications

The JIS G3458 standard is formulated for heat-resistant alloy steel pipes used as high-temperature fluid conveying pipes for heaters and boiler tubes.

Production Method:

Grade Heat treatment
STPA 12 Low temperature annealing isothermal annealing, full annealing, normalizing full annealing, normalizing or normalizing followed by tempering
STPA 20
STPA 22
Low temperature nnealing, isothermal annealing, full annealing or followed tempering
STPA 23
STPA 24
Isothermal annealing, full annealing or normalizing followed by tempering
STPA 25
STPA 26

Chemical Composition:

Grade Chemical Composition %
C Si Mn P S Cr Mo
STPA 12 0.10~0.20 0.10~0.50 0.30~0.80 0.035 max. 0.035 max. - 0.45~0.65
STPA 20 0.10~0.20 0.10~0.50 0.30~0.60 0.035 max. 0.035 max. 0.50~0.80 0.45~0.65
STPA 22 0.15max. 0.50 max. 0.30~0.60 0.035 max. 0.035 max. 0.80~1.25 0.45~0.65
STPA 23 0.15max. 0.50~1.00 0.30~0.60 0.030 max. 0.030 max. 1.00~1.50 0.45~0.65
STPA 24 0.15max. 0.50 max. 0.30~0.60 0.030 max. 0.030 max. 1.90~2.60 0.87~1.13
STPA 25 0.15max. 0.50 max. 0.30~0.60 0.030 max. 0.030 max. 4.00~6.00 0.45~0.65
STPA 26 0.15max. 0.25~1.00 0.30~0.60 0.030 max. 0.030 max. 8.00~10.00 0.90~1.10

Mechanical Properties:

Grade Mechanical Properties
Tensile strength Yield point or proof stress Elongation %
kgf/mm2 {N/mm2} kgf/mm2 {N/mm2} No. 11 or No.12 test piece No. 5 test piece No.4 test piece
Longitudinal Transverse Longitudinal Transverse
STPA 12 39{382}min. 21{206} min. 30 min. 25 min. 24 min. 19 min.
STPA 20 42{412}min. 21{206} min. 30 min. 25 min. 24 min. 19 min.
STPA 22 42{412}min. 21{206} min. 30 min. 25 min. 24 min. 19 min.
STPA 23 42{412}min. 21{206} min. 30 min. 25 min. 24 min. 19 min.
STPA 24 42{412}min. 21{206} min. 30 min. 25 min. 24 min. 19 min.
STPA 25 42{412}min. 21{206} min. 30 min. 25 min. 24 min. 19 min.
STPA 26 42{412}min. 21{206} min. 30 min. 25 min. 24 min. 19 min.

Casing Manufacturing Process

ASTM A36 hot rolled steel angle

ASTM A36 hot rolled steel angle

Posted: Nov 21, 2024
What is mild steel angle iron and what is it used for?

What is mild steel angle iron and what is it used for?

Posted: Nov 20, 2024
Benefits of steel sheet piles as construction material

Benefits of steel sheet piles as construction material

Posted: Nov 13, 2024
How to solve the problem of steel sheet pile corrosion in the soil?

How to solve the problem of steel sheet pile corrosion in the soil?